Items Brand | High-grade Magnesia Brick | |||||
MZ-91 | MZ-93 | MZ-95 | MZ-97 | |||
MgO | ≥ | % | 90 | 93 | 95 | 97 |
SiO2 | ≤ | – | – | 2.50 | 1.20 | |
CaO | ≤ | 3.0 | 2.50 | 2.0 | 1.50 | |
A.P | ≤ | 20 | 18 | 18 | 50 | |
CCS | ≥ | MPa | 40 | 50 | 50 | 1650 |
0.2MPa RUL | ≥ | ºC | 1500 | 1550 | 1600 | 1650 |
Items Brand | Magnesia-zirconia Brick | |||
HTMZr-I | HTMZr-II | |||
MgO | ≥ | % | 70 | 75 |
ZrO2 | ≥ | 12 | 12 | |
SiO2 | ≤ | 9.5 | 3.0 | |
CaO | ≤ | 2.0 | 6.0 | |
A.P | ≤ | 18 | 18 | |
B.D | ≥ | g/cm3 | 3.05 | 3.10 |
CCS | ≥ | MPa | 50 | 60 |
TSR (1100ºC, Water-cooling Water-cycle) | ≥ | times | 15 | 20 |
Items Brand | Direct Bonded Magnesite Chrome Brick | ||||
DMC-9A | DMC-12 | HTMGe-16 | |||
MgO | ≥ | % | 70 | 65 | 60 |
SiO2 | ≤ | 2.50 | 2.50 | 2.50 | |
Cr2O3 | ≥ | 9.0 | 12.0 | 16.0 | |
A.P | ≤ | 19 | 19 | 19 | |
CCS | ≥ | MPa | 40 | 40 | 40 |
0.2MPa RUL T0.6 | ≥ | ºC | 1600 | 1600 | 1600 |
TSR (1100ºC, Water-cooling Water-cycle) | ≥ | times | 4 | 5 | 5 |
Items Brand | Resintered Brick of Fused Magnesia | |||||
DMZ-95 | DMZ-97A | DMZ-97B | DMZ-98 | |||
MgO | ≥ | % | 95 | 97 | 96.5 | 97.5 |
SiO2 | ≤ | 1.50 | 1.0 | 1.20 | 0.80 | |
CaO | ≤ | 1.50 | 1.20 | 1.50 | 1.20 | |
A.P | ≤ | 17 | 17 | 17 | 17 | |
CCS | ≥ | MPa | 50 | 50 | 50 | 50 |
0.2MPa RUL | ≥ | ºC | 1650 | 1700 | 1700 | 1700 |