ω (Al2O3) ≥/% | 50 | 60 | 70 | 70 | 70 | 80 | 90 | |
Refractoriness /℃ | 1760 | 1780 | 1780 | 1780 | 1780 | 1780 | 1780 | |
0.2MPa Refractoriness Underload ≥/℃ | / | / | / | 1400 | 1550 | 1600 | 1650 | |
Bonding Time /s | 60-180 | |||||||
Cold Crushing Bonding Strength ≥/MPa | 110℃×24h | 1.0 | 1.0 | 1.0 | 2.0 | 2.0 | 2.0 | 2.0 |
1400℃×3h | 4.0 | 4.0 | 4.0 | 6.0 | / | / | / | |
1500℃×3h | / | / | / | / | 6.0 | 6.0 | 6.0 | |
Permanent Liner Change /% | 1400℃×3h | -5-+1 | -5-+1 | -5-+1 | -5-+1 | / | / | / |
1500℃×3h | / | / | / | / | -5-+1 | -5-+1 | -5-+1 | |
Grain Size /% | <1.0mm | 100 | ||||||
>0.5mm | 2 | |||||||
<0.074mm | 50 | 50 | 50 | 50 | 50 | 40 | 40 |